Thermanit 25/14 E-309L TIG rod
Classifications high-alloyed
EN ISO 14343-A: AWS A5.9:
W 23 12 L ER309L
Characteristics and field of use
Stainless wet corrosion up to 350 °C (662 °F). Well suited for depositing intermediate layers when
welding cladded materials. Favourably high Cr- and Ni-contents, low C content. For joining unalloyed/
low-alloy steels/cast steel grades or stainless heat resistant Cr-steels/cast steel grades to austenitic
steels/cast steel grades. For depositing intermediate layers when welding the side of plates clad with
low-carbon – non-stabilized and stabilized – austenitic CrNi(MoN) austenitic metals.
Marks (rods0nly)
W 23 12 L / ER309L
Base materials
TüV-certified parent ns between 1.4583 – X10CrNiMoNb18-12
and ferritic steels up to S355N. Joints of and between high-tensile, unalloyed and alloyed
quenched and tempered steels, stainless, ferritic Cr and austenitic Cr-Ni steels, high manganese
steels as well as claddings: for the first layer of chemical resistant weld claddings0n ferriticpearlitic
steels up to fine grained structural steels S500N, in steam boiler and pressure boiler construction,
as well as creep resistant fine grained structural steels 11NiMoCr4-7 acc. to leaflet “SEW-Werkstoffblatt”
No. 365, 366, 20MnMoNi5-5 and G18NiMoCr3-7.
Typical composition of welding rod (Wt-%)
C Si Mn Cr Ni
0.02 0.5 1.7 24.0 13.0
Mechanical properties of all-weld metal
Heat Treatment Yield strength
0.2% Tensile strength Elongation
(L0=5d0)
Impact values
in J CVN
MPa MPa % +20°C:
untreated 430 580 30 80
Operating data
Polarity = – Shielding gas (EN ISO 14175):
I1
Dimensions (mm)
1.6 2.0 2.4 3.2
Approvals and certificates
TüV (2661.), CWB (ER 309L-Si), GL (4332)